¿Aún no es miembro de TradeKey.com? Regístrese para conectarse con 9 millones de importadores y exportadores a nivel mundial. registro |
BOOK A CALL
Book Call On Your Favorite Time
Code
🗘

By Signing Up. I agree to TradeKey.com Terms of Use, Privacy Policy, IPR and receive emails related to our services

Contact Us
product
Prev
breathable freely plastic runway breathable freely plastic runway breathable freely plastic runway breathable freely plastic runway
Next

breathable freely plastic runway

|

- Minimum Order

País:

China

N º de Modelo:

-

Precio FOB:

Lugar de origen:

-

Precio de pedido mínimo:

-

Cantidad de pedido mínimo:

-

Detalle de embalaje:

under customer's requirement

El tiempo de entrega:

-

Capacidad de suministro:

-

Tipo de pago:

-

Grupo de productos :

-

Contactar ahora
Miembro Básico

Persona de contacto Ms. Olivia

Han Kow north Road, Wuhan, Hubei

Contactar ahora

Especificaciones del producto

Descripción del producto

 

Construction Technology Process of Breathable freely plastic runway



1、In order to ensure bottom coating's perviousness, we should avoid construction in a condition of burning sun or under higher temperature(>**0℃). If there is dew on the morning, it is not fit for construction too. Anyway the base surface should be dry before construction.

2、To clean the base surface, and do waterproof treatment to concrete surface after the surface totally drying. Using a roller to paint a layer of waterproof material. The recommended coverage per square is 0.2KG.The surface curing time is *4 hours.

3、After finishing solidifying, we prepare the high elasticity black colloidal particles with particle size of **4mm, mixed with high strength PU single glue. And the recommended proportion of those is 1:8. Then after mixing well, we pour them into pover. The laying thickness is ***0mm. And the recommended dosage of particles per square is 8KG, with 1KG glue per square. The solidity time is *4 hours.

4、The proportion of finishing paint A material on runway and B material is 1:3. And mixing them well for following use. Then mixing EPDM with particle size of **2mm and finishing paint well, with proportion of 1:1, then pour them into paver. Let spray gun's angle keep *0 degree for spraying. After finishing spraying, we need *4hour for solidifying&maintenance. Spraying the runway in the opposite direction again. The recommended dosage of finishing paint is 1.2kg per square, EPDM particles are 1.1kg per square, the catalyst is  0.**2kg per square, then it still needs *4 hours to solidify.

5、 After finishing for *4hours solidifying&maintenance, we can mark line on the ground, and the marking paint is 0.*1kg per square.

6、Finishing construction of all progress, after 7days for maintenance for the runway, we can put it into use.

 

País: China
N º de Modelo: -
Precio FOB: Obtener el precio más reciente
Lugar de origen: -
Precio de pedido mínimo: -
Cantidad de pedido mínimo: -
Detalle de embalaje: under customer's requirement
El tiempo de entrega: -
Capacidad de suministro: -
Tipo de pago: -
Grupo de productos : -

Send a direct inquiry to this supplier

A:

Ms. Olivia < GUANGZHOU GREENWALK SPORTS PLASTIC MATERIAL CO., LTD. >

quiero saber: