NO.18,Fudao Road, Licang District, Qingdao, Shandong
Specification:
Appearance: cream powder
Size: **0 mesh
Chloride: 0.*5% max
Moisture: *5% max
Viscosity: ******0 cps
Ph: **8
Ash content: ****7%
Calcium: 1% max
Welding grade sodium alginate use in welding rods:
Coatings are applied to welding rods or electrodes to act as a
flux and to control the conditions in the immediate vicinity of the
weld, such as temperature or oxygen and hydrogen availability. The
dry ingredients of the coating are mixed with sodium silicate
(water glass) which gives some of the plasticity necessary for
extrusion of the coating onto the rod and which also acts as the
binder for the dried coating on the rod. However the wet silicate
has no binding action and does not provide sufficient lubrication
to allow effective and smooth extrusion. An additional lubricant is
needed, and a binder which will hold the damp mass together before
extrusion and maintain the shape of the coating on the rod during
drying and baking. Alginates are used to meet these
requirements.
b. The quantities of alginates used The quantities of
alginates used are very dependent on the type of welding rod being
coated and the extrusion equipment being used. For soluble
alginates it may be 0.**1.2% or low-hydrogen welding rods and
0.***0.*5% for acid and organigc types. For the thixotropic
alginates, manufacturers often find it more effective to use a
mixture of calcium alginate and sodium alginate with a total
alginate content of 0.**0.6% for low hydrogen electrodes.